LOCTITE STYCAST US 2350
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Main features
- Flame retardent
- Low CTE
- Room temperature curing
Product Description
LOCTITE STYCAST US 2350 is a flexible, flame retardant, mineral-filled, polyurethane compound. This potting compound has long pot life, and is low viscosity so it flows well and adheres to many substrates. It has very low odor and does not contain TDI or mercury compounds.
LOCTITE STYCAST US 2350 has a mixing ratio 1:4 by volume and cures at room temperature.
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Density (g)Density (g)
1.4 g/cm3Mix RatioMix Ratio
21.2:100Work life @25°CWork life @25°C
0.75 hoursThermal Properties
UL 94 RatingUL 94 Rating
V2Electrical Properties
Surface ResistivitySurface Resistivity
1540000000000000 Ohms/sqVolume ResistivityVolume Resistivity
61200000000000 Ohms⋅cmChemical Properties
Water AbsorptionWater Absorption
0.09 %Additional Information
Recommended Curing Conditions
- 12 to 24 hours @ 23 °C
Alternate Cure Schedule
- 1 to 3 hours @ 65 to 85°C