LOCTITE STYCAST PC62

Main features

  • Fluorescent under UV
  • Toluene free
  • Easily removable with soldering iron

Product Description

LOCTITE® STYCAST PC 62 conformal coating is a rapid-drying acrylic for circuit board protection applications. This colorless material is fluorescent under UV light and as a toluene-free alternative, it provides solid environmental and mechanical protection.

LOCTITE® STYCAST PC 62  with its superior toughness and abrasion resistance can operate in temperatures ranging from -40 to 125°C. It is easily removable with a soldering iron or suitable solvent and is typically used for Printed circuit boards.

Advantages of Loctite Stycast PC 62

  • Fluorescent under UV light
  • Toluene-free
  • Superior toughness and abrasion resistance
  • Easily removable

Cure Schedule

  • 24 hours @ 25°C , in an oven
  • 45 minutes @ 75°C
Product Family

STYCAST PC62

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 96 days
CA Shipping in 12 weeks
EU Shipping in 60 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Film ThicknessFilm Thickness
25-100 µm
Specific GravitySpecific Gravity
0.82
Electrical Properties
Dielectric StrengthDielectric Strength
78 kV/mm
Volume ResistivityVolume Resistivity
1.04x10^16 Ohms⋅cm
Physical Properties
ViscosityViscosity
52 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers