LOCTITE STYCAST E2534FR
Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

Main features
- Flame retardant
- Halogen free
- High thermal conductivity
Product Description
LOCTITE STYCAST E 2534 FR epoxy potting compound complies with recent demands on environmentally friendly products and does not contain brominated flame retardants. It is a two-component epoxy that can be used in a 100:4 ratio with catalysts such as CAT 9. It can achieve a continuous operating temperature of -40 to 130°C and an intermittent of -40 to 150°C.
LOCTITE STYCAST E 2534 FR can be used with a variety of catalysts. For more information on mixed properties when used with other available catalysts, please contact your local technical service representative for assistance and recommendations.
Recommended Cure Schedule
- 16 to 24 hours @ 25°C or
- 2 hour @ 65°C
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Chemical Properties
Physical Properties
Additional Information
What is the difference in viscosity if we use different catalysts?
- CAT 9 TDS mentions only part A having 350.000 cPs, and no mixed viscosity (estimated around 33.000 cPs)
- CAT 24LV TDS mentions only the MIXED viscosity around 3.300 cPs, resulting in about 10 times lower viscosity vs CAT 9