LOCTITE EDAG PM 406V1 E&C
Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

Main features
- High conductivity
- High solids content
- Hot air dry cure
Product Description
LOCTITE EDAG PM406V1 E&C is a screen printable, conductive ink formulated to have very high conductivity and solids content. It can be used on PET, paper and PVC substrates.
LOCTITE EDAG PM406V1 E&C can operate in operating temperature up to 100°C that has high solids content and dries fast. It is typically used for printed circuitry, RFID and other conductive circuits.
Recommended Drying Cycle
- 30 minutes @ 90°C or
- 15 minutes @ 120°C
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Density (g)Density (g)
3 g/cm3SolidsSolids
79 %Physical Properties
ViscosityViscosity
21,600 mPa.s