LOCTITE EDAG 461SS E&C
Harmonization Code : 32159090 | Printing ink, writing or drawing ink, and other inks, whether or not concentrated or solid, specifically for those classified as other within that category

Main features
- Conductive
- Screen printable
- Dries at low temperatures
Product Description
LOCTITE EDAG 461SS E&C conductive ink is designed for display applications on ITO film. It consists of very finely divided silver particles dispersed in a thermoplastic resin.
LOCTITE EDAG 461SS E&C is a screen printable and extremely flexible polyester resin with a butyl cellosolve acetate. It is typically used on ITO coated films, membrane switches, digitizers and flexible circuits with a maximum operating temperature of 149°C
Cure Schedule
- 30 minutes @ 71°C or
- 15 minutes @ 93°C or
- 5 minutes @ 121°C
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
SolidsSolids
75 %Physical Properties
ViscosityViscosity
17,000 mPa.s