LINQBOND UF3550R | Reworkable Underfill

Main features

  • Low stress, high fatigue and crack resistance
  • Low viscosity, solvent-free
  • Fast cure

Product Description

UF3550R is a reworkable one-component epoxy adhesive designed for electronic device bonding. It is easy to use and suitable for various electronic components, including casting and sealing. This resin cures quickly at high temperatures, reducing working time and increasing efficiency simultaneously.

UF3550R forms tough, strong structural bonds with excellent shear, peel, and impact strength. The resin's durability is exceptional, passing numerous environmental tests. When used for underfilling CSP and BGA chips, it buffers the expansion and contraction stress of solder ball contacts and mitigates the shear force generated by reaction forces during drop tests.

Cure Schedule

  • 80 °C for 30 min 
  • 100 °C for 15 min 
  • 150 °C for 3 min
Product Family

LINQBOND UF3550R

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 16 weeks
CA Shipping in 16 weeks
EU Shipping in 16 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot LifePot Life
168 hours
Specific GravitySpecific Gravity
1.16
Work life @25°CWork life @25°C
168 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
35 °C
Electrical Properties
Volume ResistivityVolume Resistivity
4.5E15 Ohms⋅cm
Physical Properties
ViscosityViscosity
550-850 mPa.s

Additional Information

Instructions for Use:

  1. Before use, thaw the product to reach room temperature for 1–2 hours. The syringe should be placed vertically while thawing. Keep the container airtight until room temperature is reached.

  2. Ensure the surface to be bonded is clean and free of contaminants like dirt, grease, or mold release agents. A simple solvent wipe is often sufficient.

  3. Cure time may vary based on the actual part geometry, material volume, and equipment. It is recommended to test on actual parts and equipment.

  4. For large-scale applications, consider a staged curing process: start with a lower temperature pre-cure, followed by a full cure at a higher temperature to effectively manage heat release.

  5. Cool down gradually after curing to minimize thermal stress.

  6. The epoxy cannot be refrozen once exposed to room temperature.

 

Rework Process:

  1. Component Removal. Component solder joints must be heated above their reflow temperature (260°C to 280°C). At this temperature, the underfill will be soft and easy to remove. The component may then be pulled or removed by twisting or with a use of a vacuum pick-up nozzle.
  2. Site Preparation. After component removal, cleaning of residues may be done by the following methods

    • Scraping. Heat the site to 250°C to 300°C and scrape off the underfill carefully avoiding damage of pads on the substrate. Alternatively, heating can also be done from the bottom of the substrate.

    • Rotating Brush. Apply a sufficient amount of pressure onto the brush to clean the residues. Care should be taken to avoid damage to the substrate.

  3. Component Replacement. Isopropanol or a flux pen may be used to ensure no residue remains on the circuit board after cleaning. Brush solder paste or flux on the board and align the new component using a vacuum and reflow using hot air. Underfill will likewise be applied followed by the cure step.

 

Storage and Handling

Store and transport below -5°C Temperature. Keep away from moisture and heat sources. It is strictly forbidden to store in outdoor environments.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers