LINQBOND SMA3602 | SMT Chipbonder

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LINQBOND SMA3602 | SMT Chipbonder

Main features

  • solvent-free
  • low stress
  • low water absorption

Product Description

LINQBOND SMA3602 is a one-component epoxy developed for chip bonding. This product offers medium viscosity, high thixotropy, and fast curing at low temperatures. It is suitable for screen printing and dispensing applications. The product forms strong cured shapes without stringing or slumping, even at high-speed dispensing and with very small dots. The hardened surface of this product does not exhibit surface oiliness.

Once cured, LINQBOND SMA3602 offers excellent adhesive strength, electrical insulation properties, and superior chemical and solvent resistance. Stable adhesive strength can be achieved with various SMT (Surface-Mount Technology) applications. This product is well-suited for electronic device encapsulation and chip bonding.

Product Family

LINQBOND SMA3602

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 16 weeks
CA Shipping in 16 weeks
EU Shipping in 16 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Red liquid
Pot LifePot Life
168 (7days) hours
Specific GravitySpecific Gravity
1.35
Thermal Properties
Degradation temperatureDegradation temperature
337 °C
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
125 °C
Specific Heat CapacitySpecific Heat Capacity
4.56 J/(g⋅°C)
Thermal ConductivityThermal Conductivity
0.3 W/m.K
Electrical Properties
Dielectric StrengthDielectric Strength
22 kV/mm
Surface ResistivitySurface Resistivity
4.5 × 10(E14) Ohms/sq
Volume ResistivityVolume Resistivity
4.5×10(E15) Ohms⋅cm
Chemical Properties
Water AbsorptionWater Absorption
0.23 %
Physical Properties
Thixotropic indexThixotropic index
>2.5
ViscosityViscosity
70000 - 120000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers