LINQBOND PM-WD310 | Two part epoxy potting material

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LINQBOND PM-WD310 | Two part epoxy potting material

Main features

  • Good moisture resistance
  • Excellent thermal shock resistance
  • Low outgassing

Product Description

LINQBOND PM-WD310 is a two-component epoxy for auto lamp and electronic device casting. LINQBOND PM-WD310 exhibits outstanding stability when subjected to various environmental tests, including resistance to moisture, chemicals, and other harsh conditions.

LINQBOND PM-WD310  ensures long-term performance and reliability in diverse settings, making it an excellent choice for applications requiring robust, reliable, and high-performance epoxy solutions, particularly in the automotive and electronics industries.

Cure schedules

  • 7 days at 25°C
  • 1 hr at 80°C
Product Family

LINQBOND PM-WD310

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Black
Mix RatioMix Ratio
2:1
Specific GravitySpecific Gravity
1.165
Thermal Properties
Degradation temperatureDegradation temperature
280 °C
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
51 °C
Thermal ConductivityThermal Conductivity
0.3 W/m.K
Weight Loss @ 300°CWeight Loss @ 300°C
5.1 %
Electrical Properties
Surface ResistivitySurface Resistivity
500000000000000 Ohms/sq
Volume ResistivityVolume Resistivity
5000000000000000 Ohms⋅cm
Mechanical Properties
ElongationElongation
5 %
Chemical Properties
Water AbsorptionWater Absorption
0.41 %
Physical Properties
ViscosityViscosity
4400-6600 mPa.s

Additional Information

.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers