LINQBOND PM-1231BK | Two part black epoxy potting material

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

LINQBOND PM-1231BK | Two part black epoxy potting material

Main features

  • High resistance against weathering, aging, and UV radiation
  • Non-corrosive, insulating, moisture-proof, and shock-resistant
  • Solvent-free, environmentally friendly, and low in carbon footprint

Product Description

LINQBOND PM-1231BK is a two-component potting epoxy designed for casting, bonding, and sealing electronic components. It boasts outstanding aging and moisture resistance, excellent electrical insulation, high hardness, and a high breakdown voltage. Moreover, PM-1231BK offers customizable viscosity to meet application requirements. Additionally, PM-1231BK offers exceptional weather, UV, and shock resistance, while remaining non-corrosive and environmentally friendly.

LINQBOND PM-1231BK is well-suited for potting high power electronic components and modules that require high heat dissipation and flame retardancy. LINQBOND PM-1231BK is the opaque version of LINQBOND PM-1231.

 

Product Family

LINQBOND PM-1231BK

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Chemistry TypeChemistry Type
Epoxy
Density (g)Density (g)
1.8 g/cm3
Mix RatioMix Ratio
5:1
Pot LifePot Life
1 hours
Thermal Properties
Operating TemperatureOperating Temperature
-40 - 90 °C
Thermal ConductivityThermal Conductivity
0.7 W/m.K
UL 94 RatingUL 94 Rating
V-0
Electrical Properties
Dielectric StrengthDielectric Strength
>25 kV/mm
Volume ResistivityVolume Resistivity
1200000000000000 Ohms⋅cm
Chemical Properties
Moisture absorptionMoisture absorption
0.15 %

Additional Information

Processing Instructions

  1. Before potting, make sure the surface is clean. Remove any oil or dust.
  2. Mix component A and B according to specified ratio. Stir thoroughly to ensure uniformity while preventing air to be introduced into the mixture. Automatic mixing and filling machine can be used. Scrape the sides of the container to ensure even mixing until the color is consistent throughout.
  3. Use the mixture within 30 minutes.
  4. Allow the potted workpiece cure at room temperature until the surface is dry. Full curing typically occurs within 48 hours. The curing process is influenced by temperature variations; generally, higher temperatures result in faster curing, while lower temperatures lead to slower curing.

Precautions for Use

  1. Before use, thoroughly mix Part A. Stratification may occur during long-term storage due to its high specific gravity. Mixing ensures consistent product performance. Do this in a well-ventilated area.
  2. Use all of the mixed Part A and B at once. Seal and store any components for future use.
  3. Typically, keep the potting thickness within 30mm. For deeper potting, contact the manufacturer for guidance.

Please note that the provided information is based on available data and typical conditions. For specific applications and detailed test results, refer to the actual test data and conduct appropriate certifications.

Storage and Handling

The product can withstand long-term exposure to fresh water, sewage, waste water, calcium carbonate aqueous solution, detergent, low-acid, and corrosive water solutions. It has short-term resistance to mineral oil, vegetable oil, fat, and fuel. However, it is not resistant to organic solvents, paint thinners, high-concentration acids, or alkalis.

Store in a ventilated, dry, and clean environment at 10–30 °C. Keep away from fire and heat sources. It is strictly forbidden to store in outdoor environments. At proper storage conditions, Part A and Part B has a shelf life of 6 months. Shelf life can be extended by using cold storage.

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers