LINQBOND DA-8410 | Die-Attach

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LINQBOND DA-8410 | Die-Attach

Main features

  • High Thermal Conductivity
  • High Reliability
  • Pressureless sintering

Product Description

LINQBONDTM DA-8410 is a silver sintering die attach paste with excellent adhesion on bare Cu substrates, as well as other metal plated substrates. Pressureless sintering is achieved at 250 °C, providing excellent adhesion and leaving no organic residues, resulting in high thermal conductivity and reliability.

LINQBONDTM DA-8410 is designed as a die attach material for applications requiring high thermal and electrical conductivity. Typically used for high thermal resistance assemblies such as LEDs, laser diodes, RF devices, automotive electronics, and power devices.

Product Family

LINQBOND DA-8410

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
24 hours
Thermal Properties
Thermal ConductivityThermal Conductivity
250 W/m.K
Physical Properties
Thixotropic indexThixotropic index
5.9
ViscosityViscosity
40000 mPa.s

Additional Information

Cure schedule

Two-Step Curing Conditions (refer to the diagram below):

  • 1st step: 5 °C/min ramp to 80 °C and hold for 30 min

  • 2nd step: 5 °C/min ramp from 80 °C to 250 °C and hold for 60 min

  • Cool down: 5 to 10 °C/min cool down to room temperature

cure schedule DA-8410

Precautions for Use

  1. Allow the container to reach room temperature before use. Syringe should be placed vertically while thawing. Thaw process for 10 cc syringe takes 1 hour.

  2. The adhesive cannot be refrozen once exposed to room temperature.

  3. To ensure uniform and stable viscosity, syringe can be placed in planetary mixer for 2 min at 800 rpm.

  4. Please note that the provided information is based on available data and typical conditions. For specific applications and detailed test results, refer to the actual test data and conduct appropriate certifications.

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers