LINQALLOY SW-SAC305 | Solder Wire

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

LINQALLOY SW-SAC305 | Solder Wire

Main features

  • Leadfree Solder Wire
  • Lowest cost Sn/Ag/Cu Alloy
  • Excellent Fatigue Resistance

Product Description

LINQALLOY SW-SAC305 solder wire is a lead-free Tin/Silver/Copper alloy that contains 96.5% Tin (Sn), 3% Silver (Ag), and 0.5% Copper (Cu) and is often written as Sn96.5Ag3.0Cu0.5. SAC305 Solder Wire is the least expensive of the two industry standard lead-free solder wires (the other being SAC405) and is used by companies working with BGA, CSP, LBGA, PBGA and CBGA components who have made the transition to Lead-free (Pb-free) soldering.

LINQALLOY SW-SAC305 solder wire presents a highly reliable solution for various soldering applications, leveraging its superior composition and performance characteristics. Comprising 96.5% tin, 3% silver, and 0.5% copper, this solder wire offers a balanced blend of properties optimized for exceptional solder joint integrity and longevity.

With a melting temperature of approximately 217-220°C, SAC305 solder wire ensures efficient and precise soldering operations across a wide range of electronic assembly processes. Its carefully engineered formulation promotes excellent wetting and flow properties, facilitating uniform solder joint formation and minimizing the risk of solder defects such as voiding and bridging.

Features:

  • Lowest Cost Sn/Ag/Cu Alloy
  • Excellent Fatigue Resistance
  • Compatible with all Flux Types
  • Excellent Solder Joint Reliability
  • Best Wetting Sn/Ag/Cu Alloy
Product Family

LINQALLOY SW-SAC305

1. Select Thickness
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Thickness.
TDS, SDS & Technical Documents

Technical Specifications

Other Properties
RoHS CompliantRoHS Compliant
Yes
General Properties
Alloy CompositionAlloy Composition
Sn96.5Ag3.0Cu0.5
Alloy TypeAlloy Type
SAC305
Specific GravitySpecific Gravity
7.4g/cc

Additional Information

Each spool has a clear label on the lid specifying the solder wire diameter as well as a label on the front identifying the alloy type, the date of manufacture, and the product lot (or batch) number. This batch number is also tied to a certificate of conformance that is also provided with the solder wires and ensures the SAC305 solder wires meet the following quality criteria:

  • Tin (Sn): 96.5%
  • Silver (Ag): 3%
  • Copper (Cu): 0.5%
  • Melting Temperature (Solidus): 217°C
  • Melting Temperature (Liquidus): 219°C
  • Spheroid Tolerance : Within 1.5%

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers