WS360 | Wax Conditioning Sheets
Harmonization Code : 4005.91.00.00 | Compounded rubber, unvulcanized, in primary forms or in plates, sheets or strip: Plates, sheets, and strip

Main features
- Good Workability
- Not water soluble
- Mild odor and fume
Product Description
WS360 Wax Conditioning Sheets are used to protect the mold surface and ensure a good releasing effect after cleaning. It is a waxing sheet that provides an ideal balance between great mold protection and high workability and it can be used for Green and non Green EMC as well as manual and auto molding processes.
WS360 performs well in a wide range of molds being able to withstand a torque of 2.9 lb-in to 18 lb-in and has a curing time of ~ 250-350 seconds. WS360 offers great workability and fume time that lasts ~10seconds. Need wax rich solutions? Contact us for additional information.
WS360 Wax Conditioning Sheets are highly effective as a protection and release product. They have good flow characteristics which enable them to reach into the mold corners and thin gate areas easily. An additional advantage is that you will need no dummy lead frame or preheating. Used in combination with our RCS Rubber Cleaning Sheets, the short mold waxing and cleaning time will lead to reduced costs and will increase your overall efficiency and productivity.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Additional Information
Compatible Working Conditions
| Clamp pressure | 30-150 Ton |
| Mold temperature | 160 - 190°C |
| Curing time | 250-350 Seconds |
| #of shots | 1-2 Shots |
CHEMLINQ WS360 wax protection and release sheets protect mold surfaces and ensure an excellent releasing effect after cleaning the mold. They are extremely well suited for production lines that work with Electromagnetic Compatibility (EMC) and provide optimal protection of molds used in the semiconductor industry for products such as as integrated circuits, diodes, transistors, and LEDs in both physical and chemical mechanisms.
Storage and packaging
The wax conditioning and release sheets come in one size that will fit a variety of molds, so you can use one waxing product for all your molds. Other dimensions are possible per customer request if the quantity allows it.
CHEMLINQ conditioning sheets come prepackaged in PE bags and in 10Kg carton boxes. They need to be stored and transferred in a cool environment and their work life is 4 days after removal from the storage conditions.
Shelf life is 12 months from manufacturing date. Stored at 5°C or below (not frozen)