RCS 880 | Rubber Cleaning Sheets
Harmonization Code : 4005.91.00.00 | Compounded rubber, unvulcanized, in primary forms or in plates, sheets or strip: Plates, sheets, and strip

Main features
- Great releasing properties
- No leadframe required
- Excellent for vents and cavities
Product Description
RCS 880 Rubber cleaning sheets are used to eliminate pollutants and stains formed on the mold surface. They perform well in a wide range of molds and are able to withstand up to 100t. These sheets offer an good cleaning performance with less smell and fumes.
RCS 880 sheets have good flow characteristics which enable them to clean mold corners and thin gate areas easily. Unlike melamine cleaners, RCS cleaning sheets can even clean the air ventilation areas without causing mold abrasion or corrosion. At the same time there's no need for dummy lead frame or preheating, something that reduces cleaning time and leads to improved production time results and productivity.
RCS 880 Rubber cleaning sheets can remove contamination of molds used in the semiconductor industry for products such as as integrated circuits, diodes, transistors, and LEDs in both physical and chemical mechanisms.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Additional Information
Difference between RCS 620 and RCS 880
RCS 880 have higher elastomer content (55%) compared to RCS 620 (40-50%) which makes it more flexible/elastic thus enabling it to reach corners and complex portions of the mold while cleaning.
In addition, RCS 880 has more concentrated cleaning ability since it has no solvent in the composition while RCS620 have additional propylene glycol compound that act as a solvent/plasticiser.
|
Recommended Application Setting |
RCS 620 & 880 |
|
Mold Pressure |
1600 – 1800 psi or 50 – 120 tons |
|
Mold Temperature |
150 – 185 ° degree celcius |
|
Curing Time |
150 – 600 seconds |
|
No of Shots |
4 to 8 shots |
Storage and packaging
These rubber sheets should be kept in room temperature. Their shelf life in these storage conditions is 9months.
They are packaged in PE bags and come in 10Kg (net) boxes. Exact width is not stated since the sheets can be arrayed for the application and width is adjusted to the box size to accommodate the net weight.
Sheet dimensions
| Sizes (in mm) | Tolerances (in mm) | |
| Length | 230 | ±5 |
| Width | 15 | ±2 |
| Thickness | 5 | ±1 |
Warning