PIT2S-DCD | 2 mil Die Cut Polyimide (Kapton) Tape with Silicone Adhesive | Single Sided Discs

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

2 mil Die Cut Polyimide Tape Silicone Adhesive Single Sided | Discs

Main features

  • Good chemical resistance
  • Good solvent resistance
  • 11,000V Breakdown Voltage

Product Description

LINQTAPE PIT2S-DCD-Series is a 2-mil, pressure sensitive silicone adhesive high-temperature resistant polyimide tape designed for both permanent and temporary bonding in many high temperature applications. These applications are can be found in semiconductor, smartcard, electronic, automotive and general manufacturing industries.

LINQTAPE PIT2S-DCDSeries Tape provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It can be used in applications that may see temperatures up to 260C. The tape can be delivered in a range of die cut discs sizes with diameters ranging from 1/8" to 12".

Product Family

LINQ PIT2S-DCD

1. Select Diameter
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Diameter.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive LayerAdhesive Layer
Silicone
Adhesive ThicknessAdhesive Thickness
38.1 µm
Chemistry TypeChemistry Type
Polyimide
ColorColor
Amber
Film ThicknessFilm Thickness
50.8 µm
Release LinerRelease Liner
None
Single or Double-Sided AdhesiveSingle or Double-Sided Adhesive
Single-Sided
Special LayerSpecial Layer
None
Total ThicknessTotal Thickness
88.9 μm
Thermal Properties
Temperature ResistanceTemperature Resistance
260 ˚C
Other Properties
RoHS CompliantRoHS Compliant
Yes
VOC-Free (100% solids content)VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion StrengthAdhesion Strength
25 Oz/in
ElongationElongation
55 %
Tensile Strength (Thin Film)Tensile Strength (Thin Film)
90 N/cm
Electrical Properties
Breakdown VoltageBreakdown Voltage
>11000 V
Volume ResistivityVolume Resistivity
10000000000000 Ohms⋅cm

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel