Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT1N-C | 1-mil Clear Polyimide (Kapton) Film

Main features

  • 1mil Optically Clear Polyimide
  • No Adhesive
  • 6000 V Breakdown Voltage

Product Description

LINQTAPE PIT1N-C is a Clear Kapton, Polyimide film whose high-performance, flexible, high-temperature resistant polyimide film is used for many high-temperature applications. Polyimide is preferred over polyester for many high temperature applications. These applications include but are not limited to semiconductor, smartcard, electronic, automotive and general manufacturing industries.

LINQTAPE PIT1N-C optically clear polyimide film is made from high-quality polyimide resin, which provides excellent mechanical, thermal, and chemical properties. This film is extremely durable and can withstand high temperatures up to 400°C without compromising its optical clarity or performance.

The optically clear nature of this film makes it perfect for use in applications where visual clarity is essential. Its transparency allows for good light transmission, making it an excellent choice for displays, touchscreens, and other optical components. Additionally, the film's high clarity makes it a suitable option for use in optical sensors and imaging systems, where precise visual information is critical. Beyond its optical properties, our optically clear polyimide film also provides excellent thermal stability, making it ideal for use in high-temperature environments. Its thermal conductivity is excellent, which allows it to dissipate heat effectively, making it an excellent option for thermal management applications.

LINQTAPE PIT1N-C is available in a range of thicknesses, widths, and lengths to meet your specific application needs. It is easy to handle, cut, and process, making it a versatile option for a wide range of industrial and consumer applications.

Product Family

LINQ PIT1N-C

1. Select Width
2. Select Length
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 2 weeks
CA Shipping in 2 weeks
EU Shipping in 2 weeks
Packaging
Please select Width and Length.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Clear
Total ThicknessTotal Thickness
25.4 μm
Electrical Properties
Breakdown VoltageBreakdown Voltage
6000 V
Mechanical Properties
ElongationElongation
40 %

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers