PIT0.5S-DCD | 0.5 mil Die Cut Polyimide (Kapton) Tape with silicone adhesive| Single Sided Discs

Harmonization Code : 3919.90.80.99 | Polyacrylic plates / sheets / film / tape / strip, self-adhesive, in rolls

PIT0.5S-DCD | 0.5 mil Die Cut Polyimide (Kapton) Tape with silicone adhesive| Single Sided Discs

Main features

  • 0.5 mil polyimide film
  • Silicone Adhesive
  • Die cut discs

Product Description

LINQTAPE PIT0.5S-DCD is a 0.5-mil, ultra thin Kapton HN Film with Silicone adhesive whose high performance, flexible, high-temperature resistant polyimide films are used for many demading applications. Polyimide is preferred over polyester for high temperature applications. These applications include but are not limited to semiconductor, smartcard, electronic, automotive and general manufacturing industries.

LINQTAPE PIT0.5S-DCD Series Film provides an excellent balance of electrical, mechanical, thermal, and chemical properties over a wide range of temperatures. It can be used in applications that may see temperatures up to 260°C (400°F).

LINQTAPE PIT0.5S-DCD polyimide tape can be delivered in a range of die cut disc sizes with diameters ranging from 1/8" to 12".

Product Family

LINQ PIT0.5S-DCD

1. Select Diameter
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Diameter.

Technical Specifications

General Properties
Adhesive LayerAdhesive Layer
Silicone
Adhesive ThicknessAdhesive Thickness
25.4 µm
Chemistry TypeChemistry Type
Polyimide
ColorColor
Amber
Film ThicknessFilm Thickness
12.7 µm
Release LinerRelease Liner
None
Single or Double-Sided AdhesiveSingle or Double-Sided Adhesive
Single-Sided
Special LayerSpecial Layer
None
Total ThicknessTotal Thickness
38.1 μm
Thermal Properties
Temperature ResistanceTemperature Resistance
260 ˚C
Electrical Properties
Breakdown VoltageBreakdown Voltage
>3000 V
Volume ResistivityVolume Resistivity
100000000000000 Ohms⋅cm
Other Properties
RoHS CompliantRoHS Compliant
Yes
VOC-Free (100% solids content)VOC-Free (100% solids content)
Yes
Mechanical Properties
Adhesion StrengthAdhesion Strength
12 Oz/in
ElongationElongation
25 %
Tensile Strength (Thin Film)Tensile Strength (Thin Film)
10 N/cm

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers