KESTER R562 Solder Paste

Harmonization Code : 3810.10.00 | Soldering, brazing or welding powders and pastes consisting of metal and other materials

KESTER R562 Solder Paste

Main features

  • Reduces BGA voiding
  • 12-hour stencil life
  • Consistent printing

Product Description

KESTER R562 is an organic acid, water-soluble solder paste specifically designed for resistance to environmental extremes.  Water-soluble pastes tend to dry out in low relative humidity and slump at high relative humidity. R562 will maintain its print characteristics, tack and activity even after exposure to environmental extremes.

Product Key Features

  • Reduces BGA voiding
  • 12-hour stencil life
  • Print speeds up to 6 in/sec
  • Consistent printing

Applications

  • Stencil printing & enclosed head printing (90% metal)
Product Family

KESTER R562

1. Select Alloy Type
2. Select Particle Size
3. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
Shipping in 6 weeks
Packaging
Please select Alloy Type, Particle Size and Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy TypeAlloy Type
Sn63Pb37, Sn62Pb36Ag2

Additional Information

Reflow Profile

The recommended reflow profile for R562 made with either the Sn63Pb37 or Sn62Pb36Ag02 is shown here. This profile is simply a guideline. Since R562 is a highly active solder paste, it can solder effectively over a wide range of profiles. Your optimal profile may be different from the one shown based on your oven, board and mix of defects. Please contact us if you need additional profiling advice.

Peak Temp: 219–230 °C

Zones:

  • Soaking Zone: 170–180 °C, 60–90 sec typical
  • Reflow Zone: 6–75 sec typical

Time to Peak Temperature: 3.5–6 min typical

Ramp-up: <1.5 °C/sec

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers