KESTER 2166-BN Soldering Flux
Harmonization Code : 29051200 | Propan-1-ol (propyl alcohol) and propan-2-ol (isopropyl alcohol)

Main features
- Halide-free formulation
- Superior surface insulation resistance
- Easy residue removal
Product Description
Kester 2166-BN is a halide-free, organic flux designed for automated soldering of circuit board assemblies. It provides excellent activity on bare copper and solder-coated boards while ensuring easy residue removal and superior compatibility with solder resists.
Product Key Features
- Contains no chlorides, bromides, phosphates, or highly corrosive materials
- Effective on both bare copper and solder-coated boards
- Outperforms typical water-soluble fluxes, ideal for SMT assemblies
- Works well with solder resists compared to other water-soluble fluxes.
Applications
- for high-speed, automated assembly lines.
- Provides reliable soldering for advanced surface mount (SMT) electronic assemblies.
- also ideal for bare copper & solder-coated boards
Packaging
Please select Package Type.
Technical Specifications
General Properties
SolidsSolids
31 %Specific GravitySpecific Gravity
1.144