Hysol MG33F-0661 | Gold Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

MG33F-0661 Gold Epoxy Mold CompoundMG33F-0661 Gold Epoxy Mold Compound

Main features

  • Environment friendly molding compound
  • Very low moisture absorption
  • Identical to MG33F-0660

Product Description

Hysol MG33F-0661 is a gold, semiconductor-grade epoxy molding compound or duroplast designed for the encapsulation and protection of tantalum capacitors. Because of its fast cure, it is also very well suited for the manufacture of reed relays.

Hysol MG33F-0661 was formulated with a short gel time to make it useful for automolding tantalum capacitors and reed relays.It is an environmentally friendly "green" molding compound which contains no bromine, antimony or phosphorus flame retardant. MG33F-0661 molding compound was developed specifically for the encapsulation of tantalum capacitors in automold applications. MG33F-0661 meets UL 94 V-0 Flammability at 6.35mm thickness.

You might be wondering, "But what's the difference between this one and MG33F-0660?" Short answer. Nothing. Back in the day, SKUs were not ideal so this is a customer specific SKU for the exact same product. Why is this here then? Maybe you ARE that customer looking for it. You are welcome.

 

Product Family

HYSOL MG33F-0661

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
4. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size, Pellet Weight and Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Gold
Filler ContentFiller Content
72 %
Specific GravitySpecific Gravity
1.81
Chemical Properties
Moisture absorptionMoisture absorption
0.42 %
Physical Properties
Spiral Flow @ 175°CSpiral Flow @ 175°C
27 cm
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
164 °C
Thermal ConductivityThermal Conductivity
0.8 W/m.K
UL 94 RatingUL 94 Rating
V0
Electrical Properties
Dielectric StrengthDielectric Strength
37 kV/mm
Volume ResistivityVolume Resistivity
2600000000000000 Ohms⋅cm
Curing Conditions
Transfer PressureTransfer Pressure
40 - 80 kg/cm2
Transfer TimeTransfer Time
5 - 10 s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers