HumiSeal Acrylic Gel Conformal Coating

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

HumiSeal Acrylic Gel Conformal Coating

Main features

  • Thixotropic
  • Fast-drying
  • Easy repairability

Product Description

HumiSeal Acrylic Gel is a fast-drying, single-component acrylic paste engineered for precision and high-build protection. Its thixotropic nature means it stays in place upon application but flows under pressure, making it the perfect companion for standard acrylic conformal coatings. It provides a rugged barrier against moisture and environmental contaminants while remaining easy to rework.

Product Key Features

  • Designed as a thick paste that will not slump or run, allowing for precise placement on vertical surfaces or specific components.
  • Rapid evaporation of solvents speeds up production throughput and allows for quicker handling of assemblies.
  • Easily removed with solvents or a soldering iron, making it ideal for boards requiring field service.

Applications

  • Used to create a physical perimeter (a "dam") on a PCB to prevent liquid conformal coatings from flowing into restricted areas like connectors or test points.
  • Effectively seals the base of large components to prevent moisture ingress or "wicking" underneath parts.
Product Family

HUMISEAL AG

1. Select Package Size
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 6 weeks
Packaging
Please select Package Size.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Density (g)Density (g)
0.95 g/cm3

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers