LOCTITE ECCOBOND FP4655

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LOCTITE ECCOBOND FP4655

Main features

  • Low stress
  • Fine particle filler
  • Combine with FP4451

Product Description

LOCTITE ECCOBOND FP4655 is a high-performance fill encapsulant that can be used alone as a cavity fill material, or in combination with FP4451 material as part of a dam and fill system. This low stress, self levelling epoxy has been used for Medical applications.

LOCTITE ECCOBOND FP4655 is based on the same chemistry as the FP4451 and, therefore, is completely compatible with that product. Its low viscosity and fine particle filler size make it ideal for devices with fine-pitch wire spacing. Dam and fill materials should be co-cured to obtain the best results.

Recommended Cure Schedule

  • 15 minutes @ 110°C plus 30 minutes @ 165°C
  • 30 minutes @ 125°C plus 90 minutes @ 165°C
Product Family

ECCOBOND FP4655

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 94 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot LifePot Life
11 hours
Specific GravitySpecific Gravity
1.88
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
150 °C
Electrical Properties
Volume ResistivityVolume Resistivity
50000000000000 Ohms⋅cm
Physical Properties
ViscosityViscosity
140,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers