PEAM-645 High Tg Polyester Acrylate/Methacrylate

Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

PEAM-645 High Tg Polyester Acrylate/Methacrylate

Main features

  • High Tg
  • Low CTE
  • High adhesion to various substrates

Product Description

PEAM-645 is a polyester acrylate/methacrylate that exhibits low CTE, high Tg, and high modulus. The oligomer has very high thermal stability and low volatility. It can be used as a base resin in a formulation or as an additive. It exhibits good adhesion on various substrates. The oligomer also exhibits good hydrolytic stability

PEAM-645 is recommended for use as a base resin in adhesive applications or coating applications. The material if used alone can exhibit brittleness and the incorporation of a toughener (such as ABS, or hyperbranched polyester) is recommended. The oligomer has good solubility in both aliphatic and aromatic co-monomers. PEAM-645 is more akin to epoxies with the smaller molecular weight (still big compared to most epoxies but much smaller than the PEAM-1044) and with higher Tg as a result. It common to mix these product for optimal results.

Product Family

DMI PEAM-645

1. Select Package Type
Price starting from €246.02
Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Amber Liquid
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
160 °C
Weight Loss @ 300°CWeight Loss @ 300°C
3 %
Physical Properties
ViscosityViscosity
5,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers