MM-204 High Tg Mono-Functional Acrylate Monomer
Harmonization Code : 2916.12 | Unsaturated acyclic monocarboxylic acids and their anhydrides, halides, peroxides, peroxyacids, and their derivatives


Main features
- Hydrolytically resistant
- Low Viscosity
- High Glass Transition Temperature (Tg)
Product Description
MM-204 dicyclopentadiene acrylate is a mono-functional acrylate monomer. It has low shrinkage and a high glass transition temperature upon cure. The secondary ester linkage is resistant to hydrolysis.
MM-204 is recommended for use as a reactive diluent for UV or peroxide cured resins, coatings or adhesives. It can also be used to improve stereolithographic processes for high-temperature applications.
Highlights
- Low viscosity
- Hydrolytically resistant
- High glass transition temperature
- Diluent for thermoset resins
- Low cure shrinkage
- High Tg
Typical Physical and Chemical Properties
PROPERTY METHOD RESULT
- Appearance at Room Temperature: Light tan liquid
- Viscosity @ 25°C (typical): 50 cPs using Haake Rheometer
- Functionality:1
- Molecular Weight: 204 daltons
- Recommended Storage: At 5°C or below
Packaging
Please select Package Type.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
AppearanceAppearance
Light Tan LiquidFunctionalityFunctionality
1Molecular weightMolecular weight
204 g/molOther Properties
Storage TemperatureStorage Temperature
5 °CPhysical Properties
ViscosityViscosity
50 mPa.s