A6225| Anti bleed Additive

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

A6225| Anti bleed Additive

Main features

  • Universal additive
  • Reduces bleed out on metal surfaces
  • Non halogenated

Product Description

A-6225 is a proprietary, patent-pending non-halogenated additive utilizing a monofunctional silicone together with a thiol reactive group allowing it to perform multiple functional roles. When used in metal filled and non-metal filled adhesive systems it reduces resin bleed out on a variety of surfaces such as with copper and gold traces. When used as a mold release in composite manufacturing the material imparts a residual anti-stiction silicone coating to surface of the parts.

A-6225 is co-curable in both free-radical based and traditional epoxy based polymerization systems. It can also enhance the rheological properties of various filled adhesives.

A-6225 is recommended for use as an additive to reduce resin bleed out specifically on metal surfaces. The recommended addition of the A-6225 to a formulation is between 2% - 5% weight percent of resin. It shows superior bleed control in silver filled formulations and can significantly reduce or eliminate resin bleed out in formulations that contain non-metal fillers such as silica. A-6225 may be applied up to full strength to molds or incorporated at 2 – 4% weight percent in resin formulations to provide mold release and surface anti-stiction properties.

Product Family

DMI A6225

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US No longer available
CA No longer available
EU Shipping in 2 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Colorless liquid
Density (g)Density (g)
0.98 g/cm3
FunctionalityFunctionality
1 Functional group/molecule
Molecular weightMolecular weight
1089 (estimated) g/mol
Thermal Properties
Flash PointFlash Point
153 °C
Physical Properties
ViscosityViscosity
50 mPa.s

Additional Information

Epoxy Resin Incompatibility

A6225 rely on thiol functionality to bond in and prevent bleeding. Unfortunately thiol group react with epoxy resin instead of substrate reducing or even eliminating the resin bleed functionality.

 

Molecular Weight Estimation

We do not specifically measure the M.W. for this material and instead rely on the average M.W. of the starting material and the functionality (thiol group) that makes the product.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers