EC Nanoscale Epoxy control

Harmonization Code : 3824.99.96.99 | Prepared binders for foundry moulds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included : Other : Other: Other

Main features

  • Eliminating Die Attach Epoxy bleed
  • Epoxy control in Semiconductor packaging
  • Excellent chemical bonding to many surfaces

Product Description

Aculon EC nanoscale thickness (4nm) repellency product is a surface treatment that uses it’s hydrophobicity and oleophobicity characteristics to create epoxy repellent surfaces to control the location of epoxy used in semiconductor packaging. Applications include eliminating die attach epoxy bleed, reduce underfill epoxy keep-out areas around flipchip die, and eliminating EMC mold flash contamination. Added features include: wirebondable when used on a metal wirebond pad, repels: water, oil, flux, solder paste, and many solvents. In general use, it is designed to bond to most metals and certain polymers and resists chemical and mechanical degradation

Product Family

ACULON AculonEC

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 6 weeks
CA Shipping in 6 weeks
EU Shipping in 6 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
0.98g/ml
Thermal Properties
Boiling PointBoiling Point
78 °C
Flash PointFlash Point
13.9 °C
Electrical Properties
Visible Light TransmissionVisible Light Transmission
100 %
Other Properties
Coating ThicknessCoating Thickness
2-4 nm
Physical Properties
ViscosityViscosity
2 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers