LOCTITE ABLESTIK QMI538NB

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK QMI538NB

Main features

  • PTFE filled
  • No bleed
  • Lower modulus than QMI536NB

Product Description

LOCTITE ABLESTIK QMI538NB is a PTFE filled non-conductive die attach paste designed for applications which require very low stress and robust mechanical properties. This low modulus (100MPa) product is used for MEMS and die stacking, with NB standing for No Bleed.

LOCTITE ABLESTIK QMI538NB is a hydrophobic BMI Hybrid product that offers low viscosity and reduced resin bleed, along with stability at higher temperatures. With its excellent adhesive strength and good popcorning resistance after solder reflow temperatures it is typically used on solder resist, flexible tapes and on bare siliconE and die passivation.

Cure Schedule

  • 30 minutes @ 175°C
  • 60 minutes @ 150°C
Product Family

ABLESTIK QMI538NB

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Pot LifePot Life
24 hours
Specific GravitySpecific Gravity
1.34
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
-70 °C
Physical Properties
Thixotropic indexThixotropic index
5
ViscosityViscosity
8,200 mPa.s

Additional Information

QMI538NB is a lower modulus alternative of QMI536NB for MEMS and die stacking from the beginning. 

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers