LOCTITE ABLESTIK ICP 8118

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK ICP 8118

Main features

  • Snap cure
  • Excellent flexibility
  • High speed dispensing

Product Description

LOCTITE ABLESTIK ICP 8118  is an electrically conductive adhesive designed for applications that require a very fast cure at low temperatures. It is ideally suited for high throughput photovoltaic dispense processes and applications where high adhesion strength is desired. Low and stable contact resistance is achieved on noble metallization during reliability testing.

LOCTITE ABLESTIK ICP 8118 is a single component acrylate that displays excellent flexibility and is typically used for flexible interconnect in photovoltaic shingle applications.

 

Snap Cure

  • 10 to 15 seconds @ 150°C
Product Family

ABLESTIK ICP8118

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 40 days
CA Shipping in 12 weeks
EU Shipping in 25 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific GravitySpecific Gravity
1.9
Electrical Properties
Volume ResistivityVolume Resistivity
0.004 Ohms⋅cm

Additional Information

Protip
By applying a flat and thin 100-200um layer using JET dispensing or STENCIL printing (instead of one domed dot), we believe that the flow out and bleeding can be reduced by lower gravity forces.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers