LOCTITE ABLESTIK 8387BM

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE ABLESTIK 8387B

Main features

  • Fast cure
  • 2 in 1
  • Die attach and Glob top

Product Description

LOCTITE® ABLESTIK 8387BΜ non conductive epoxy die attach adhesive has been formulated for use in high throughput die attach applications. It has been used for the glass attach of Optical and 3D sensors and has been successfully used for lid attach in aerospace and defence applications. This non conductive adhesive can be used as an encapsulant and has black pigmentation for blocking stray light. It can be used to bond Nickel-plated surfaces on FR4.

LOCTITE® ABLESTIK 8387BΜ is a low temperature cure material that has the unique ability to be a 2 in 1 solution for both die attach and glob top encapsulation applications.

 

Cure Schedule

  • 1 hour @ 100°C
  • 90 minutes @ 90°C
Product Family

ABLESTIK 8387BM

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 37 days
CA Shipping in 12 weeks
EU Shipping in 35 days
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
48 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
122 °C
Physical Properties
Thixotropic indexThixotropic index
4,5
ViscosityViscosity
9,200 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers