LOCTITE ABLESTIK 8361J

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

LOCTITE ABLESTIK 8361J

Main features

  • Excellent dispensability
  • 1mil Spacers
  • Minimal voiding

Product Description

LOCTITE ABLESTIK 8361J die attach epoxy adhesive is designed for high reliability packaging applications. This electrically conductive epoxy offers high purity and minimal resin bleed, together with a low amount of condensable volatiles. 

LOCTITE ABLESTIK 8361J exhibits minimal tailing and stringing, along with minimal voiding. It stands out for its excellent strength retention after temperature and humidity exposure and its moderate stress absorption properties. Please note that this product contains 1mil silver spacers for a more controlled bondline.

Cure Schedule

  • 1 hour @ 175°C
  • 30 minute ramp to 115°C + 30 minutes @ 175°C
Product Family

ABLESTIK 8361J

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 30 days
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
24 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
40 °C
Weight Loss @ 300°CWeight Loss @ 300°C
0.3 %
Chemical Properties
Moisture absorptionMoisture absorption
0.65 %
Physical Properties
Thixotropic indexThixotropic index
4.5
ViscosityViscosity
9,000 mPa.s

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers