LOCTITE ABLESTIK 561K

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

LOCTITE ABLESTIK 561K

Main features

  • Reworkable
  • Flexible
  • Thermally conductive

Product Description

LOCTITE ABLESTIK 561K is a white epoxy film designed for substrate attach and heat sink bonding. This adhesive film is designed for bonding materials with severely mismatched coefficients of thermal expansion. All data and results will vary with different thicknesses.

LOCTITE ABLESTIK 561K is a reworkable assembly film that passes NASA outgassing standards. If you require a low temperature cure  you can consider LOCTITE ABLESTIK 566K. It is mainly used for substrate attach and heat sink bonding and has a glass fabric carrier.

 

Cure Schedule

  • 30min @150°C
  • 2 hours @ 125°C
Product Family

ABLESTIK 561K

1. Select Package Type
2. Select Thickness
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 20 days
CA Shipping in 12 weeks
EU Shipping in 45 days
Packaging
Please select Package Type and Thickness.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Work life @25°CWork life @25°C
4392 hours
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
55 °C
Thermal ConductivityThermal Conductivity
0.9 W/m.K
Weight Loss @ 300°CWeight Loss @ 300°C
0.34 %
Electrical Properties
Volume ResistivityVolume Resistivity
9100000000000 Ohms⋅cm
Chemical Properties
Moisture absorptionMoisture absorption
0.9 %
Water Extract pHWater Extract pH
8

Additional Information

How does ABLESTIK 561K compares to ABLESTIK 566K?

The storage temperature of both materials is as low as -40 °C to guarantee its material properties over a longer range of time.
The 561K is a great reference material that can be stored at -40 °C for 12 months but can also be stored at ambient (25 °C) for up to 6 months without loss of performance.
The difference with 561K however, in the higher minimum cure schedule of 125 °C for 2 hours.
The 566K material  can cure at 100 °C but this is achieved by an increased catalyst load making the material more reactive, giving it shorter shelf life. (We would expect -20 °C storage to be sufficient for the 566K for 3-6 months)


Essentially you end up with two options:

  • Use 561K with 6 months storage at 25 °C and accept a higher 125 °C cure
  • Use 566K with 3-6 months storage at -20 °C and cure at 100 °C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel