LOCTITE ABLESTIK 561

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

LOCTITE ABLESTIK 561

Main features

  • Amber epoxy film
  • Flexible & Reworkable
  • Thermally conductive

Product Description

LOCTITE ABLESTIK 561 is designed for bonding materials with mismatched coefficients of thermal expansion. In many bonding applications, components may be repaired. This thermally conductive epoxy film is typically used for Assembly applications.

LOCTITE ABLESTIK 561 is reworkable, meaning that components glued with this adhesive can be debonded by heating the assembly to 150°C and sliding a thin blade, such as a razor blade, between the bonded surfaces. This adhesive is also available in a low temperature cure version.

 

Cure Schedule

  • 30min @150°C
  • 2 hours @ 125°C
Product Family

ABLESTIK 561

1. Select Package Type
2. Select Thickness
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type and Thickness.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
50 °C
Thermal ConductivityThermal Conductivity
0.3 W/m.K
Weight Loss @ 300°CWeight Loss @ 300°C
0.71 %
Electrical Properties
Dielectric StrengthDielectric Strength
39370 kV/mm
Volume ResistivityVolume Resistivity
5000000000000 Ohms⋅cm

Additional Information

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers