ABchimie526UV LED Soft Dual Cure Conformal Coating
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

Main features
- One Component
- Dual Cure (UV and Humidity)
- Low Viscosity
Product Description
ABChimie® 526UV LED is a transparent urethane acrylate conformal coating designed to provide mechanical and environmental protection to electronic components and assemblies. It features dual-cure technology (UV LED and humidity), which allows for the complete crosslinking through the entire PCB, even in areas that may be covered by shadow. The coating also allows the PCB to be soldered through without producing toxic gases.
ABChimie 526UV LED exhibits a low viscosity formulation and can be applied by brush, pad printing, manual spray, and selective coating. The decreased viscosity allows for a very thin thickness of 80-100 microns. The coating cures rapidly under UV LED light (395 nm), has no VOCs, and can be applied to high-speed manufacturing processes to increase productivity. ABChimmie 526UV is in full compliance with REACH and RoHS regulations, and has UL94 V0 and UL746E (QMJU2-E308681) certifications.
Product Key Features
- Transparent, thin coverage
- Dual Cure (UV LED + Humidity)
- Thin film thickness (80 - 100 microns)
- Excellent adhesion to PCBs
- Resists mold growth
- Fast UV LED cure for high volume production
- No VOCs
- Brush, Spray, Printing, Selective Coating (ideal) applications
- UL94 V0 and UL746E
Applications
- Conformal coating for Printed circuit assemblies.
- Protection for plastic casings or covers.
- Protection for optically clear applications ex. lenses.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Electrical Properties
Thermal Properties
Physical Properties
Additional Information
Frequently Asked Questions About ABChimie® 526 UV LED
What are typical applications for ABChimie® 526 UV LED?
ABChimie® 526 UV LED is a UV-curable conformal coating designed to protect printed circuit board assemblies (PCBs) and components in demanding manufacturing environments, including:
- Automotive electronics (e.g., control units, sensors)
- Industrial automation (e.g., motor drives, PLCs)
- Consumer electronics (e.g., smart devices, wearables)
- Other high-reliability electronic assemblies
Should I control the application environment?
ABChimie® 526 UV led should be applied at a minimum temperature of 16°C and a minimum relative humidity of 50% are recommended for coating application. The relative humidity of at least 50% is recommended for the second ABchimie TDS ABchimie 526 UV and UV LED polymerization mechanism. Before applying, the printed circuit board must be clean, dry, and free of moisture. A stage in an oven at 80 °C for 4 hours is usually sufficient.
Learn More About ABChimie® 526 UV LED
ABChimie® 526 UV LED is a proven solution for engineers seeking fast, reliable protection of electronic assemblies in demanding manufacturing environments. This UV-curable conformal coating delivers rapid curing, excellent electrical insulation, and strong environmental resistance—ideal for applications in automotive electronics, industrial automation, consumer electronics, and other high-reliability assemblies.
Main Advantages of ABChimie 526 UV LED
ABchimie® 526 UV LED cures through a dual mechanism: UV exposure initiates rapid surface curing, while moisture ensures complete curing throughout the coating. This combination provides a uniform, durable protective layer with optimal adhesion and performance.
ABChimie® 526 UV LED provides excellent mechanical protection. This hardness helps resist scratches, abrasion, and minor impacts, ensuring long-term stability of encapsulated components.
ABchimie® 526 UV LED can be soldered through without generating highly toxic gases, ensuring safe processing. The coating maintains its integrity during soldering, allowing reliable connections while protecting the underlying components.
ABchimie® 526 UV LED provides excellent adhesion even in harsh environments. The coating forms a durable, long-lasting protective layer that resists moisture, chemicals, and temperature variations, ensuring reliable performance under demanding conditions.
How to Choose a Conformal Coating
Selecting the most suitable resin requires consideration of key factors:
- ✔ Norms & Compliance
- ✔ Environment / Exposure Conditions
- ✔ Repairability
- ✔ Electrical Performance
- ✔ Application Method
- ✔ Operating Temperature
Compliance You Can Trust ✅
ABChimie® 526 UV LED meets stringent industry standards, ensuring reliability and regulatory adherence for OEMs and contract manufacturers:
- REACH Compliant
- RoHS 2011/65/EU Compliant
UL94 V0
UL746E (QMJU2-E308681)
Curing Tip: ABChimie 526 UV LED cures with UV rays. It is crucial to use the appropriate equipment, as well as the recommended settings, to achieve the best properties of the resin.
Ref. Leistung / ref power ln % over wavelength in nm
Key Curing Properties for 526 UV LED DS55 and 526 UV LED DS140
LED
395 nm
3000 mJ/cm2
Coating Thickness
100 μm
Minimum UVA Power
500 mW/cm2
Typical property values shown for reference only and should not be used as specifications.
How to Optimise for the Best Results
PCBs must be completely dry and thoroughly clean, with no dust, grease, wax, or other contaminants. Coating adhesion depends directly on the quality of the substrate. All flux residues must be fully removed, as they can become corrosive and lead to circuit malfunctions.
For cleaning equipment or removing uncured ABchimie 526 UV or UV LED varnish, we recommend using SND or ABclean solvent (no aqueous solutions).
It is essential to use the correct UV equipment (UV or LED) and follow the recommended settings to achieve the optimal properties of the cured conformal coating. These parameters influence both the coating’s reactivity and surface quality. ABchimie526UV and UV LED cure through UV exposure, with moisture contributing to a secondary curing mechanism.

Curing Mechanism: UV light creates the first cure, and after 7 days the moisture from the environment completes the curing process.
How does Moisture Cure Work?
During UV curing, exposure to UV light activates the photoinitiators in the conformal coating, triggering rapid polymerization of the resin. This results in an immediate surface cure and fast development of handling strength. UV curing provides precise, on-demand curing in exposed areas, enabling high-throughput processing while maintaining coating uniformity.
ABchimie526UV and ABchimie526UV LED use the same dual curing mechanism to ensure complete curing, including in shadowed or hard-to-reach areas. Initial curing is achieved by UV exposure, while a secondary moisture-activated cure completes the process at ambient temperature. For full curing in shaded areas, a minimum relative humidity of 50% is required for at least 7 days.
ABChimie 526 UV is also available in the mercury lamp version, which cures with an mercury lamp.
ABChimie 526 UV [Go to 526 UV Product Page↗]
- Conformal Coating
- Fluorescent under UV light
- Excellent adhesion to flexible substrates
- Dual curing with UV exposure and moisture curing
Best suited for: High-speed process looking to use LED light for curing